A nanoindentation study of the viscoplastic behavior of pure lithium

Producción científica: Articlerevisión exhaustiva

77 Citas (Scopus)

Resumen

Applying mechanical stresses is a possible approach to suppress dendrite and mossy lithium (Li) in Li metal electrodes. We conducted, in this work, nanoindentation tests on pure Li metal in an argon-filled glove box to study its viscoplastic behavior at room temperature. Both load-controlled and strain rate-controlled nanoindentations showed clear viscoplastic characteristics of Li. Based on an iterative finite element (FE) modeling approach, we determined a viscoplastic constitutive law for Li. In addition, we demonstrated by FE modeling that elastic modulus, on the order of GPas, has a negligible influence on the nanoindentation response of Li at ambient temperature.

Idioma originalEnglish
Páginas (desde-hasta)191-195
Número de páginas5
PublicaciónScripta Materialia
Volumen130
DOI
EstadoPublished - mar 15 2017

Nota bibliográfica

Publisher Copyright:
© 2016 Acta Materialia Inc.

Financiación

This work is supported by the National Science Foundation under Cooperative Agreement No. 1355438.

FinanciadoresNúmero del financiador
U.S. Department of Energy Chinese Academy of Sciences Guangzhou Municipal Science and Technology Project Oak Ridge National Laboratory Extreme Science and Engineering Discovery Environment National Science Foundation National Energy Research Scientific Computing Center National Natural Science Foundation of China1355438

    ASJC Scopus subject areas

    • General Materials Science
    • Condensed Matter Physics
    • Mechanics of Materials
    • Mechanical Engineering
    • Metals and Alloys

    Huella

    Profundice en los temas de investigación de 'A nanoindentation study of the viscoplastic behavior of pure lithium'. En conjunto forman una huella única.

    Citar esto