Resumen
Nanoporous palladium nickel (np-PdNi) was produced by dealloying PdNi alloy thin films. The pore and ligament dimensions were reduced by 50% when surfactants were added to the sulfuric acid etching solution. Changes in film composition and biaxial film stress were used to track the dealloying evolution in the surfactant-modified etching solution. Ultrasonic agitation was also used to enhance dealloying and shortened the required time from 5 h to 1 h, while retaining a pore/ligament size of ∼5 nm.
| Idioma original | English |
|---|---|
| Páginas (desde-hasta) | 167-169 |
| Número de páginas | 3 |
| Publicación | Scripta Materialia |
| Volumen | 62 |
| N.º | 3 |
| DOI | |
| Estado | Published - feb 2010 |
Nota bibliográfica
Funding Information:This material is based upon work supported by the National Science Foundation under Grant No. DMR-0847693 . Acknowledgment is made to the Donors of the American Chemical Society Petroleum Research Fund (Grant No. 43324-G10 ), for support of this research.
Financiación
This material is based upon work supported by the National Science Foundation under Grant No. DMR-0847693 . Acknowledgment is made to the Donors of the American Chemical Society Petroleum Research Fund (Grant No. 43324-G10 ), for support of this research.
| Financiadores | Número del financiador |
|---|---|
| National Science Foundation (NSF) | 0847693, DMR-0847693 |
| American Chemical Society Petroleum Research Fund | 43324-G10 |
ASJC Scopus subject areas
- General Materials Science
- Condensed Matter Physics
- Mechanics of Materials
- Mechanical Engineering
- Metals and Alloys
Huella
Profundice en los temas de investigación de 'Achieving finer pores and ligaments in nanoporous palladium-nickel thin films'. En conjunto forman una huella única.Citar esto
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver