Resumen
We examined the use of differential scanning calorimetry (DSC) to measure the specific heat anomalies at second-order charge-density-wave transitions in blue bronze (K0.3MoO3), NbSe3 and TaS3. Samples of different morphologies were investigated to examine possible effects of different thermal time constants; results were generally independent of morphology. For blue bronze, an anomaly Δcp = 0.16R was found at its 180 K transition; for NbSe3, Δcp = 0.06R at 142 K, and for TaS3, Δcp < 0.03R at 220 K. Our results demonstrate the practicality of using DSC for the quantitative measurement of small specific heat anomalies ({greater-than or approximate}0.2%) in synthetic metals.
| Idioma original | English |
|---|---|
| Páginas (desde-hasta) | 307-316 |
| Número de páginas | 10 |
| Publicación | Synthetic Metals |
| Volumen | 46 |
| N.º | 3 |
| DOI | |
| Estado | Published - mar 1992 |
Nota bibliográfica
Funding Information:We greatlya ppreciateth e technicaal ssistanceo f Guy Lehman,h elpful commentsb y George Mozurkewicha nd help in sample preparationa nd characterizatiobny Gary Minton. This researchw as funded in part by the NationalS cienceF oundationG, rantNos. DMR-86-15463a ndDMR-89-15440, and by the Mabel Pew Myrin Trust.
Financiación
We greatlya ppreciateth e technicaal ssistanceo f Guy Lehman,h elpful commentsb y George Mozurkewicha nd help in sample preparationa nd characterizatiobny Gary Minton. This researchw as funded in part by the NationalS cienceF oundationG, rantNos. DMR-86-15463a ndDMR-89-15440, and by the Mabel Pew Myrin Trust.
| Financiadores |
|---|
| US NationalS cienceF oundationG |
ASJC Scopus subject areas
- Electronic, Optical and Magnetic Materials
- Condensed Matter Physics
- Mechanics of Materials
- Mechanical Engineering
- Metals and Alloys
- Materials Chemistry
Huella
Profundice en los temas de investigación de 'Differential scanning calorimetry at charge-density-wave transitions'. En conjunto forman una huella única.Citar esto
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver