Ir directamente a la navegación principal Ir directamente a la búsqueda Ir directamente al contenido principal

Sliding wear of non-hydrogenated diamond-like carbon coatings against Al, Cu and Ti

Producción científica: Conference contributionrevisión exhaustiva

Resumen

Magnetron sputtered non-hydrogenated diamond-like carbon (DLC) coatings were tested against Al, Cu and Ti pins using a vacuum pin-on-disc tribometer. The objective was to compare Al, Ti, and Cu transfer to DLC coatings in air (29% RH) and an inert atmosphere (argon). In argon, a significant amount of adhesion and material transfer occurred from the Al and Ti pins to the DLC coating surfaces inflicting severe damage to the coatings. Wear and material transfer of the DLC coating against Cu were negligible in argon. Compared to tests in argon, the tribological performance of the DLC coatings against Al and Ti improved significantly in ambient air. In contrast, the wear rate of the DLC coatings against Cu was much higher in ambient air compared to that in argon.

Idioma originalEnglish
Título de la publicación alojadaProceedings of the World Tribology Congress III - 2005
Páginas491-492
Número de páginas2
DOI
EstadoPublished - 2005
Evento2005 World Tribology Congress III - Washington, D.C., United States
Duración: sept 12 2005sept 16 2005

Serie de la publicación

NombreProceedings of the World Tribology Congress III - 2005

Conference

Conference2005 World Tribology Congress III
País/TerritorioUnited States
CiudadWashington, D.C.
Período9/12/059/16/05