We report a method of making nanowires of bismuth (Bi) with diameters ranging from 30 to 200 nm and lengths up to several millimeters. The nanowires are extruded spontaneously at the rate of a few micrometers per second at room temperature from the surfaces of freshly grown composite thin films consisting of Bi and chrome-nitride. The high compressive stress in these composite thin films is the driving force responsible for the nanowire formation. This mechanism can also be used to create nanowires of other materials.
| Idioma original | English |
|---|---|
| Páginas (desde-hasta) | 3248-3250 |
| Número de páginas | 3 |
| Publicación | Applied Physics Letters |
| Volumen | 81 |
| N.º | 17 |
| DOI | |
| Estado | Published - oct 21 2002 |
ASJC Scopus subject areas
- Physics and Astronomy (miscellaneous)
Huella
Profundice en los temas de investigación de 'Stress-induced growth of bismuth nanowires'. En conjunto forman una huella única.Citar esto
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver